Low-Zinc Silicon Brass, UNS C87600, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Silicon Brass, ASTM B584; ASTM B198-13C
Material Notes: Recommended Casting Methods: Sand. Applications: Valve stems. Classified under: Silicon bronzes and silicon brasses. ASTM B584; formerly ASTM B198-13C. <>Alloy does not respond to heat treating. Typical data for as-sand-cast separately cast test bars (M01 temper).
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Strength
- Machinability
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|