Tombasil, UNS C87800, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Silicon Brass, ASTM B176; ASTM ZS144A
Material Notes:
Casting methods recommended for this alloy: die. Applications: Bearings, gears, impellers, rocker arms, valve stems, brush holders, bearing races, small boat propellers. Classified under: Silicon bronzes and silicon brasses. ASTM B584; formerly ASTM B198-13B Typical data for separately cast test bars. Alloy does not respond to heat treating. Casting shrinkage allowance is 1.9%
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Creep Strength
- Modulus of Elasticity
- Compressive Strength
- Charpy Impact
- Fatigue Strength
- Machinability
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
- Annealing Temperature
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|