Tin Bronze, UNS C90500, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Bronze; Copper Casting Alloy
Key Words: Tin Bronze, G Bronze, ASTM B22; ASTM B584; ASTM B22-D; ASTM B143-1A
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Continuous, Investment, and Sand. Applications: Bearings and bushings, pump impellers, valve components, seal rings, steam fittings, gears. Classified under: Silicon bronzes and silicon brasses. ASTM B22; ASTM B584; formerly ASTM B22-D; ASTM B143-1A Alloy does not respond to heat treating
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Strength
- Izod Impact
- Fatigue Strength
- Machinability
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|