Leaded Tin Bronze, UNS C92300, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Leaded tin bronze, ASTM B584; ASTM B143-2B
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Continuous, and Sand. Applications: Valves, pipe fittings, and high-pressure steam castings. Superior machinability to C90300. Classified under: Leaded tin bronzes. ASTM B584; formerly ASTM B143-2B Data typical for sand-cast test bars. Alloy does not respond to heat treating
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Strength
- Izod Impact
- Machinability
- Electrical Resistivity
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|