High-Leaded Tin Bronze, UNS C93600, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Close Analogs: Information provided by Spectrum Machine, Inc.
Key Words: MIL-C-22229 (sand cast)
Material Notes: Typically used for bearings and bushings. Good suitability for soldering and brazing. Not recommended for oxyacetylene, gas shielded, or coated metal welding.
| Available Properties |
- Density
- Hardness, Brinell
- Elongation at Break
- Modulus of Elasticity
- Machinability
- Electrical Resistivity
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Melting Point
- Solidus
- Liquidus
- Processing Temperature
|
|
|
|