High-Leaded Tin Bronze, UNS C93700, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: High lead tin bronze, ASTM B22, ASTM B584, ASTM B22-C, ASTM B144-3A
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, and Sand. Applications: Bearings for high speed and heavy pressures, pumps, impellers, corrosion-resistant applications, pressure tight castings. Classified under: High-leaded tin bronzes. ASTM B22; ASTM B584; formerly ASTM B22-C; ASTM B144-3A Typical data for sand cast test bars. Alloy does not respond to heat treating. Casting shrinkage allowance is 2%
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Creep Strength
- Compressive Strength
- Charpy Impact
- Izod Impact
- Fatigue Strength
- Machinability
- Electrical Resistivity
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|