High-Leaded Tin Bronze, UNS C93800, Copper Casting Alloy, Centrifugally Cast
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Key Words: High lead tin bronze, ASTM B66, ASTM B584, ASTM B144-3D
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, and Sand. Applications: Bearings for general service and moderate pressures, pump impellers and bodies for use in acid mine water. Classified under: High-leaded tin bronzes. ASTM B66; ASTM B584; formerly ASTM B144-3D Typical data for chilled centrifugally cast test bars. Alloy does not respond to heat treating
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Compressive Strength
- Machinability
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|