High-Leaded Tin Bronze, UNS C94300, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: High lead tin bronze, ASTM B66, ASTM B584, ASTM B144-3E
Material Notes:
Casting methods recommended for this alloy: Centrifugal and Sand. Applications: High-speed bearings for light loads. Classified under: High-leaded tin bronzes. ASTM B66; ASTM B584; formerly ASTM B144-3E Typical data for sand-cast test bars. Alloy does not respond to heat treating. Casting shrinkage allowance is 1.5%
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Compressive Strength
- Izod Impact
- Machinability
- Electrical Resistivity
- Magnetic Permeability
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|