Aluminum Bronze, UNS C95300, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Aluminum bronze, ASTM B148, ASTM B148-9B
Material Notes: Heat treatable. Except where noted, all property values listed below are for sand casting. Recommended Casting Methods: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand. Applications: Electrical applications, pickling baskets, nuts, gears, steel mill slippers, marine equipment, welding jaws, non-sparking hardware. Classified under: Aluminum bronzes. ASTM B148; formerly ASTM B148-9B
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Compressive Strength
- Poissons Ratio
- Charpy Impact
- Izod Impact
- Fatigue Strength
- Machinability
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Elastic Limit
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|