Sluminum-Silicon Bronze, UNS C95600, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand. Applications: Cable connectors, terminals, valve stems, marine hardware, gears, worms, pole-line hardware. Classified under: Aluminum bronzes Data typical for as-sand-cast separately cast test bars (M01 temper). Alloy does not respond to heat treating
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Machinability
- Electrical Resistivity
- Specific Heat Capacity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|