Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Nickel aluminum bronze, ASTM B148
Material Notes: Alloy does not respond to heat treating. Casting shrinkage allowance is 1.6%.Recommended Casting Methods: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand. Applications: Propellers hubs, blades, and other parts in contact with salt water. Corrosion Resistance: resists salt water corrosion. Classified under: Aluminum bronzes. ASTM B148
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Compressive Strength
- Poissons Ratio
- Charpy Impact
- Fatigue Strength
- Machinability
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|