UNS C96200, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Material Notes:
Casting methods recommended for this alloy: Centrifugal and Sand. Applications: Components of items, being used for sea water corrosion resistance. Classified under: Copper-nickels Properties for as-sand-cast separately cast test bars (M01 temper). Alloy does not respond to heat treating
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Strength
- Charpy Impact
- Fatigue Strength
- Machinability
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|