Copper Nickel Tin UNS C96800, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Close Analogs: Copper content calculated as remainder.
Material Notes: This spinodal alloy is similar to the more common C96200, with higher strength. Common applications include pumps and fluid handling components for fresh or salt water.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Machinability
- Electrical Resistivity
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|