Leaded Nickel Bronze, UNS C97600, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Leaded nickel silver, ASTM B584, ASTM B149-11A
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Investment, and Sand. Applications: Marine castings, sanitary fittings, ornamental hardware, valves, pumps. Classified under: Nickel silvers. ASTM B584; formerly ASTM B149-11A Data typical for sand-cast test bars. Alloy does not respond to heat treating. Casting shrinkage allowance is 2%
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Creep Strength
- Modulus of Elasticity
- Compressive Strength
- Charpy Impact
- Fatigue Strength
- Machinability
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|