Leaded Nickel Bronze, UNS C97800, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Leaded nickel silver, ASTM B584, ASTM B149-11B
Material Notes:
Casting methods recommended for this alloy: Investment, Permanent Mold, and Sand. Applications: Ornamental and sanitary castings, valves and valve seats, musical instrument components. Classified under: Nickel silvers. ASTM B584; formerly ASTM B149-11B Typical data for sand-cast test bars. Alloy does not respond to heat treating. Casting shrinkage allowance is 1.6%
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Machinability
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|