Beryllium Copper 21C Copper Casting Alloy Solution Treated and Aged

 

Subcategory: Copper Alloy; Nonferrous Metal

Material Notes:
The 1% Co content is a good grain refiner, and as a result, this alloy is used instead of beryllium-copper alloys C82500 and C23400 when thin sections must be cast at high temperatures or when thick and thin sections are present within the same casting in order to achieve a uniform fine-grained structure. The higher cobalt content imparts better wear resistance but less desirable polishability and machinability. Typical uses are comparable to those of beryllium-copper alloys C82500 and C23400.

Test specimen: solution treated at 790 to 800°C and aged 3 hours at 345°C.

Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Machinability
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 100°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Melt Temperature
  • Solution Temperature
  • Aging Temperature
  • Casting Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。