Tin-Bearing Copper (SCuR3), 1/2 Hard Temper
Subcategory: Copper Alloy; Nonferrous Metal; Wrought Copper
Material Notes: Product forms include sheet and strip. Used in automotive radiator fins. Information taken from Nippon Mining and Metals Co. literature.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- Melting Point
- Solidus
- Liquidus
|
|
|
|