Ductile Iron grade 60-40-18
Subcategory: Ductile Iron; Alloy Cast Iron; Metal
Key Words: UNS F32800, ASTM A395-76, ASME SA395, ferritic, pressure parts
Material Notes: Carbon represents the total carbon in the above composition. Cerium is an optional constituent in ductile iron. Most ductile irons are specified based on mechanical properties and have loosely defined compositions. For example, 60-40-18 ductile iron is specified to have a minimum tensile strength of 60 ksi (414 MPa), a yield strength of 40 ksi (276 MPa) and an elongation of 18%. Ferritic, annealed. Applications include pressure-containing parts for use at elevated temperatures, valves and fittings for steam and chemical plant equipment.
| Available Properties |
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|