Ductile Iron grade 60-40-18, low temperature service

 

Subcategory: Ductile Iron; Alloy Cast Iron; Metal

Key Words: UNS F32800, ASTM A536-72, MIL-I-11466B(MR), ferritic, shock resistant parts

Material Notes:
Carbon represents the total carbon in the above composition. Cerium is an optional constituent in ductile iron. Most ductile irons are specified based on mechanical properties and have loosely defined compositions. For example, 60-40-18 ductile iron is specified to have a minimum tensile strength of 60 ksi (414 MPa), a yield strength of 40 ksi (276 MPa) and an elongation of 18%. Ferritic, may be annealed. Applications include shock resistant parts, low temperature service, machine components subject to shock and fatigue loads.

Available Properties
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。