Ductile Iron grade 65-45-12
Subcategory: Ductile Iron; Alloy Cast Iron; Metal
Key Words: UNS F33100, ASTM A536, ferritic, shock loading, fatigue loading
Material Notes: Carbon represents the total carbon in the above composition. Cerium is an optional constituent in ductile iron. Most ductile irons are specified based on mechanical properties and have loosely defined compositions. For example, 65-45-12 ductile iron is specified to have a minimum tensile strength of 65 ksi (448 MPa), a yield strength of 45 ksi (310 MPa) and an elongation of 12%. Mostly ferritic, as cast or annealed. Applications include machine components subject to shock and fatigue loads. Hardness and machinability data provided by manufacturer/supplier, Siltin Industries, Inc.
| Available Properties |
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Machinability
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|