Ductile Iron grade D7003
Subcategory: Ductile Iron; Alloy Cast Iron; Metal
Key Words: UNS F34800, pearlitic, wear resistant, selective hardening, gears
Material Notes: Carbon represents the total carbon in the above composition. Cerium is an optional constituent in ductile iron. Most ductile irons are specified based on mechanical properties and have loosely defined compositions. Pearlitic. Applications include highly stressed parts requiring very good wear resistance and good response to selective hardening, gears.
| Available Properties |
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |