Ductile Iron tension grade 120-90-02
Subcategory: Ductile Iron; Alloy Cast Iron; Metal
Material Notes: Carbon represents the total carbon in the above composition. Cerium is an optional constituent in ductile iron. Most ductile irons are specified based on mechanical properties and have loosely defined compositions. For example, 120-90-02 ductile iron is specified to have a minimum tensile strength of 120 ksi (827 MPa), a yield strength of 90 ksi (621 MPa) and an elongation of 2%. Determined for a single temperature of ductile iron, heat treated to approximate various standard grades. Properties were obtained using test bars machined from 25 mm keel blocks.
| Available Properties |
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|