High Silicon Ductile Iron at RT 4Si-0.9V nominal alloy content
Subcategory: Ductile Iron; Alloy Cast Iron; Metal
Material Notes: Subcritically annealed for 4 hours at 790°C, air cooled. Soak 3 hours at 900°C, cool to 700°C, soak 5 hours, furnace cool to below 425°C.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
|
|
|
|
| Property Data |