ASTM A439 Austenitic Ductile Iron type D4
Subcategory: Ductile Iron; Alloy Cast Iron; Metal
Material Notes: Austenitic ductile (nodular) iron at room temperature.
| Available Properties |
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
|
|
|
|