Alpha-2 Titanium Aluminide, Ti3Al
Subcategory: Intermetallic
Close Analogs: Composition table gives weight percent.
Key Words: Ti3Al
Material Notes: Intermetallic aluminides have good mechanical properties and stability to be used in high temperature environments. A thin protective Al2O3 coating forms to provide oxidative stability. A range of stoichiometries is possible through elemental substitutions. Researchers are examining titanium aluminide applications in fields such as jet engine turbines because of their high temperature properties and low density. May be cast. Difficult to process by ingot metallurgy, forging, or sheet rolling.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Melting Point
- Maximum Service Temperature, Air
- Maximum Service Temperature, Inert
- Critical Ordering Temperature
- Crystal Structure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|