Iron Aluminide, Fe3Al
Subcategory: Intermetallic
Close Analogs: Composition table gives weight percent.
Key Words: Fe3Al
Material Notes: Intermetallic aluminides have good mechanical properties and stability to be used in high temperature environments. A thin protective Al2O3 coating forms to provide oxidative stability. Crystal structures include D03 ordered BCC and B2 ordered BCC.
| Available Properties |
- Density
- Modulus of Elasticity
- Melting Point
- Critical Ordering Temperature
|
|
|
|