Pure Lead (Corroding Lead), UNS L50042, Sand Cast
Subcategory: Lead Alloy; Nonferrous Metal
Key Words: Lead Alloys
Material Notes: 99.94% min. Pb is a typical specification for pure lead. This grade is the most common in the US and is used as raw material for lead chemicals and pigments.