5% Sn Antimonial Lead Solder, UNS L54321
Subcategory: Lead Alloy; Nonferrous Metal; Solder/Braze Alloy
Key Words: Lead Alloys
Material Notes: Various specifications are possible for exact composition and impurity limits.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Elongation at Break
|
|
|
|
| Property Data |