10/90 (90Pb-10Sn) Solder - ASTM B32 Grade Sn10A, UNS L54520
Subcategory: Lead Alloy; Tin Alloy; Nonferrous Metal; Solder/Braze Alloy
Key Words: Tin Alloys; Lead Alloys
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |