58Pb-40Sn-2.0Sb Tin-Lead-Antimony Solder, ASTM Class 40C
Subcategory: Lead Alloy; Tin Alloy; Nonferrous Metal; Solder/Braze Alloy
Key Words: in Alloys; Lead Alloys
| Available Properties |
- Density
- Melting Point
- Solidus
- Liquidus
|
|
|
|