MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Magnesium AM60A-F, Die Cast

 

Subcategory: Magnesium Alloy; Nonferrous Metal

Key Words: UNS M10600; Mg; ASTM B 94; European EN 1753 MC21230 (Ingot UNS M10601)

Material Notes:
Mg content calculated as balance. Excellent energy-absorption characteristics and excellent ductility. Slightly higher strength than AM50A, but with otherwise similar properties. Applications for die casting alloy in as-cast (F) temper include parts that require good ductility and toughness with reasonable yield and tensile properties (such as automotive wheels). Should be used only where good salt water resistance is not required. Slightly lower strength but greater ductility and toughness when compared with AZ91 alloys.

Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Compressive Yield Strength
  • Poissons Ratio
  • Charpy Impact
  • Machinability
  • Shear Modulus
  • Electrical Resistivity
  • Heat of Fusion
  • CTE, linear 20°C
  • CTE, linear 100°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Casting Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。