Magnesium AM60A-F, Die Cast
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: UNS M10600; Mg; ASTM B 94; European EN 1753 MC21230 (Ingot UNS M10601)
Material Notes: Mg content calculated as balance. Excellent energy-absorption characteristics and excellent ductility. Slightly higher strength than AM50A, but with otherwise similar properties. Applications for die casting alloy in as-cast (F) temper include parts that require good ductility and toughness with reasonable yield and tensile properties (such as automotive wheels). Should be used only where good salt water resistance is not required. Slightly lower strength but greater ductility and toughness when compared with AZ91 alloys.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Poissons Ratio
- Charpy Impact
- Machinability
- Shear Modulus
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|