Magnesium AZ21X1-F, Extruded Bars and Shapes
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: UNS M11210; Mg
Material Notes: Mg content calculated as balance. Used in F-temper for battery anodes.
|
|
|