MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Magnesium AZ63A-T6, Sand Cast

 

Subcategory: Magnesium Alloy; Nonferrous Metal

Key Words: UNS M11630; Elektron AZG; Mg; Old SAE 50; AMS 4420; AMS 4422; AMS 4424; ASTM B 80; SAE J465 (Ingot UNS M11631)

Material Notes:
Sand Casting is ASTM B 80; SAE J465. Mg content calculated as balance. Good room temperature strength, ductility, and toughness. Commonly used for parts in commercial and military structural applications requiring moderate strength and good ductility and toughness. Not typically used anymore - largely superseded by AZ91.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell E
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Compressive Yield Strength
  • Ultimate Bearing Strength
  • Bearing Yield Strength
  • Poissons Ratio
  • Charpy Impact
  • Fatigue Strength
  • Machinability
  • Shear Modulus
  • Shear Strength
  • Electrical Resistivity
  • Heat of Fusion
  • CTE, linear 20°C
  • CTE, linear 100°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Casting Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。