Magnesium AZ81A-T4, Cast
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: UNS M11810; Electron A8; Mg; ASTM B 80; ASTM B 199; ASTM B 403; SAE J465; Old SAE 505; European EN 1753 MC21110 (Ingot UNS M11811)
Material Notes: Mg content calculated as balance. Sand Castings: ASTM B 80. Permanent Mold Castings: ASTM B 199. Investment Castings: B403. Readily castable, has a low microshrinkage tendency, and is used in the solution-treated condition (T4 temper). Typically used for commercial and military permanent-mold and investment castings requiring good strength and excellent ductility and toughness. Good castability tough, pressure tight.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell E
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Ultimate Bearing Strength
- Bearing Yield Strength
- Poissons Ratio
- Charpy Impact
- Fatigue Strength
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|