Magnesium AZ92A-T5, Cast
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: UNS M11920; Mg; SAE J465; Old SAE 500; AMS 4434; AMS 4453; AMS 4484; ASTM B 80; ASTM B 199; ASTM B 403 (Ingot UNS M11921)
Material Notes: Mg content calculated as balance. A, B, C, D, and E Have the same nominal composition but differ in ranges and/or specified impurity limits. Sand Casting: AMS 4434, ASTM B 80; Investment Casting: AMS 4453, ASTM B 403; Permanent Mold Casting: AMS 4484, ASTM B 199; Typically used for commercial and military pressure-tight sand and permanent-mold castings having high tensile strength and good yield strength.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell E
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Ultimate Bearing Strength
- Bearing Yield Strength
- Poissons Ratio
- Fatigue Strength
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|