Malleable iron casting, Class 40010
Subcategory: Malleable Iron; Metal
Key Words: ASTM A220, ANSI G48.2, MIL-I-1444B, Malleable iron casting grade 40010, pearlitic, martensitic
Material Notes: Pearlitic and Martensitic. Temper carbon in necessary matrix without primary cementite or graphite. Applications include general engineering service at normal and elevated temperatures. Dimensional tolerance range for castings is stipulated.
Available Properties |
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|