Malleable iron casting, Class 90001
Subcategory: Malleable Iron; Metal
Key Words: ASTM A220, ANSI G48.2, MIL-I-1444B, Malleable iron casting grade 90001, pearlitic, martensitic
Material Notes: Pearlitic and Martensitic. Temper carbon in necessary matrix without primary cementite or graphite. Applications include general engineering service at normal and elevated temperatures. Dimensional tolerance range for castings is stipulated.
| Available Properties |
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|