Malleable iron casting, Class M5003 air quenched and tempered
Subcategory: Malleable Iron; Metal
Key Words: ASTM A602, SAE J158, Malleable iron casting grade M5003, automotive, ferritic, good machinability
Material Notes: Automotive. Ferritic and tempered pearlite, may be tempered martensite for some applications. Applications include selective hardening, planet carriers, transmission gears, differential cases.
| Available Properties |
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|