Magnesium QE22A-T6, Cast
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: UNS M18220; Mg; European EN 1753 MC65210; AMS 4418; ASTM B 80; ASTM B 199; ASTM B 403 (Ingot UNS M18221)
Material Notes: Mg content calculated as balance. Nd content above refers to Nd-rich rare earths. Typically used for commercial and military sand and permanent mold castings used in the solution treated and artificially aged condition (T6 temper) with high yield strengths at temperatures up to 200°C. Castings have excellent short time elevated temperature mechanical properties and are pressure tight and weldable.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Compressive Strength
- Compressive Modulus
- Poissons Ratio
- Charpy Impact
- Fatigue Strength
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|