Magnesium QH21A-T6, Cast
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: Mg
Material Notes: Mg content calculated as balance. Nd content above refers to Nd-rich rare earths. Good castability, pressure tight, creep resistance and high yield strength to 250°C.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Poissons Ratio
- Fatigue Strength
- Machinability
- Shear Modulus
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Casting Temperature
|
|
|
|