Magnesium WE43A-T6, Sand/Permanent Mold Castings
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: UNS M18430; Mg; AMS 4427; ASTM B 80; European EN 1753 MC95320
Material Notes: Mg content calculated as balance. Typically used for military and aerospace sand castings used in the solution-heat-treated and artificially aged condition (T6 temper). Castings retain properties at elevated temperatures (under 250°C) for periods of time greater than 5000 hrs, and they are pressure tight and weldable.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|