Magnesium ZC-63A-T6, Sand/Permanent Mold Castings
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: UNS M16631; Mg; ASTM B 80; European EN 1753 MC32110
Material Notes: Mg content calculated as balance. Commercial and military sand castings used in the solution heat treated and artificially aged (T6 temper) condition. Superior properties to AZ91C-applications with better castability. Useful in pressure tight applications. Can be welded.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|