Magnesium ZE41A-T5, Cast
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: UNS M16410; Mg; AMS 4439; ASTM B 80; European EN 1753 MC35110 (Ingot UNS M16411)
Material Notes: Nd content above refers to Nd-rich rare earths. Commercial and aerospace castings used in the artificially aged condition (T5 temper) with better castability than ZK51A and good strength up to 93°C. Useful in pressure tight applications.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell E
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Compressive Strength
- Ultimate Bearing Strength
- Bearing Yield Strength
- Poissons Ratio
- Charpy Impact
- Fatigue Strength
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|