Magnesium ZE63A-T6, Cast
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: UNS M16630; Mg; ASTM B 93 (Ingot UNS M16631)
Material Notes: Nd content above refers to Nd-rich rare earths. Aerospace and military sand and investment castings used in solution heat treated and artificially aged condition (T6 temper). Has excellent castability and pressure tightness. Especially useful in thin-section castings for applications requiring high mechanical strength and freedom from porosity. Special heat treatment in hydrogen is required to develop mechanical properties, which results in a wall thickness limitation for the castings.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Compressive Strength
- Compressive Modulus
- Poissons Ratio
- Fracture Toughness
- Machinability
- Shear Modulus
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|