Magnesium ZK51A-T5, Cast
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: UNS M16510; Mg; AMS 4443; ASTM B 80; SAE J465; Old SAE 509 (Ingot UNS M16511)
Material Notes: Mg content calculated as balance. Aerospace and military sand castings used in artificially aged condition (T5 temper) with high yield strength and good ductility. This alloy is suggested for highly stressed parts that are small or relatively simple in design. Solution treatment is not required.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell E
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Compressive Strength
- Ultimate Bearing Strength
- Bearing Yield Strength
- Poissons Ratio
- Fatigue Strength
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|