Magnesium ZK61A-T5, Cast
Subcategory: Magnesium Alloy; Nonferrous Metal
Key Words: UNS M16611; Mg; AMS 4444; ASTM B 80; SAE J465; Old SAE 513 (Ingot UNS M16610)
Material Notes: Mg content calculated as balance. Typically used for simple, highly stressed aerospace and military castings of uniform cross section. High in cost. Intricate castings subject to microporosity and cracking due to shrinkage. Not readily welded. Sometimes used in T5 temper (artificially aged), but usually in the solution heat treated and artificially aged (T6) condition to develop properties fully.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Poissons Ratio
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|