60Pd-40Ag Alloy, Hard
Subcategory: Precious Metal; Nonferrous Metal; Palladium Alloy
Key Words: Palladium Silver Alloy
Material Notes: Used for precision resistance wires because of its very low temperature coefficient of resistivity.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
|
|
|
|