60Pd-40Cu Alloy, Hard Drawn
Subcategory: Precious Metal; Nonferrous Metal; Palladium Alloy
Key Words: Palladium Copper Alloy
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Electrical Resistivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |