AISI Type 303 Stainless Steel, annealed, tested at 540°C (1000°F)
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Heat Resisting; Metal
Close Analogs: AISI Type 303 Se
Key Words: T303, T 303, 303SS, 303 SS, AFNOR Z 10 CNF 18.09 (Fr), UNI X 10 CrNiS 18 09, SUS 303, SS14 2346 (Sweden), B.S. 303 S 21, UNS S30300, AMS 5640 (1), ASME SA194, ASME SA320, ASTM A194, ASTM A314, ASTM A320, ASTM A320, ASTM A473, ASTM A581, ASTM A582, MIL SPEC MIL-S-862, SAE J405 (30303), DIN 1.4305, X12CrNiS188, EN 58M, austenitic, ISO 683/13 17, 18-8
Material Notes: Short time tensile test, 115 MPa stress for 1% creep at 10,000 hours
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|